- Patent Title: Super high-strength flux cored arc welded joint having excellent impact toughness, and welding wire for manufacturing same
-
Application No.: US14651853Application Date: 2013-12-24
-
Publication No.: US10065272B2Publication Date: 2018-09-04
- Inventor: Hong-Chul Jeong , Jin-Woo Lee , Dong-Ryeol Lee , Il-Wook Han , Hong-Kil Lee
- Applicant: POSCO
- Applicant Address: KR Pohang-si
- Assignee: POSCO
- Current Assignee: POSCO
- Current Assignee Address: KR Pohang-si
- Agency: Cantor Colburn LLP
- Priority: KR10-2012-0154333 20121227; KR10-2013-0163194 20131224
- International Application: PCT/KR2013/012150 WO 20131224
- International Announcement: WO2014/104731 WO 20140703
- Main IPC: B23K35/30
- IPC: B23K35/30 ; B23K35/02 ; B23K35/362 ; B23K35/368 ; B23K9/23 ; C22C38/02 ; C22C38/04 ; C22C38/08 ; C22C38/12 ; C22C38/42 ; C22C38/44 ; C22C38/50 ; C22C38/54 ; C22C38/58 ; C22C38/00 ; C22C38/22 ; C22C38/24 ; C22C38/38 ; B23K35/36

Abstract:
An ultra high-strength flux-cored arc welded joint having excellent impact toughness comprises: 0.01 wt % to 0.06 wt % of carbon (C), 0.1 wt % to 0.5 wt % of silicon (Si), 1.5 wt % to 3.0 wt % of manganese (Mn), 2.5 wt % to 3.5 wt % of nickel (Ni), 0.5 wt % to 1.0 wt % of molybdenum (Mo), 0.4 wt % to 1.0 wt % of copper (Cu), 0.4 wt % to 1.0 wt % of chromium (Cr), 0.01 wt % to 0.1 wt % of titanium (Ti), 0.003 wt % to 0.007 wt % of boron (B), 0.001 wt % to 0.006 wt % of nitrogen (N), 0.02 wt % (excluding 0) or less of phosphorus (P), 0.01 wt % (excluding 0) or less of sulfur (S), 0.03 wt % to 0.07 wt % of oxygen (O), and remaining iron (Fe) as well as unavoidable impurities.