Method of manufacturing hot press formed part, and hot press formed part
Abstract:
A method of manufacturing a hot press formed part by hot pressing a coated steel sheet that is obtained by forming a Zn-based coating layer on a surface of a steel sheet includes: heating the coated steel sheet to a temperature range of 750° C. or more and 1000° C. or less; cooling a surface of the coated steel sheet; and hot press forming the coated steel sheet under a condition that a surface temperature of the coated steel sheet is 400° C. or less and an average temperature of the coated steel sheet is 500° C. or more or a temperature of a center position of the coated steel sheet in a thickness direction is 530° C. or more.