Abstract:
A tempered glass has a compressive stress layer in a surface thereof, includes as a glass composition, in terms of mass %, 50 to 80% of SiO2, 10 to 30% of Al2O3, 0 to 6% of B2O3, 0 to 2% of Li2O, and 5 to 25% of Na2O, and is substantially free of As2O3, Sb2O3, PbO, and F.