Process for preparation of modified polyethylene terphthalate with improved barrier, mechanical and thermal properties and products thereof
Abstract:
The present invention relates to a copolyester having intrinsic viscosity greater than 0.50 dL/gm, comprises: terephthalate polyester composition; and a modified transparent polybutylene naphthalate, wherein the modified polybutylene naphthalate comprises naphthalene dicarboxylic acid, 1,4-butane diol, and isophthalic acid or monoethylene glycol or diethylene glycol or cyclohexane dimethanol or polyethylene naphthalate, nucleating agent, and a modified nanoclay.