Cold wax dispersion process
Abstract:
A method includes grinding a wax into wax particles having a size in a range from about 600 microns to about 800 microns forming a mixture of the wax particles with water and a surfactant; and homogenizing the mixture to form a wax dispersion, the homogenizing step is maintained below about 35° C. A wax dispersion includes a wax a surfactant; and water, particles of the wax dispersion are a uniform, irregular, non-platelet morphology. A wax dispersion made by a process includes grinding a wax into wax particles having a size in a range from about 600 microns to about 800 microns, forming a mixture of the wax particles with water and a surfactant, and homogenizing the mixture to form a wax dispersion, the homogenizing step is maintained below about 35° C. and the wax has a uniform, irregular, non-platelet morphology imparted by combination of the grinding and homogenizing steps.