- Patent Title: Ultra supercritical boiler header alloy and method of preparation
-
Application No.: US16051874Application Date: 2018-08-01
-
Publication No.: US10260129B2Publication Date: 2019-04-16
- Inventor: Brian A. Baker , Gaylord D. Smith , Ronald D. Gollihue
- Applicant: Huntington Alloys Corporation
- Applicant Address: US WV Huntington
- Assignee: Huntington Alloys Corporation
- Current Assignee: Huntington Alloys Corporation
- Current Assignee Address: US WV Huntington
- Agency: Burris Law, PLLC
- Main IPC: C22C19/05
- IPC: C22C19/05 ; C22F1/10 ; F22B37/22

Abstract:
A high temperature, high strength Ni—Co—Cr alloy is provided. The alloy includes, in weight percent (wt. %): 23.5 to 25.5% Cr, 15.0 to 22.0% Co, 1.1 to 2.0% Al, 1.0 to 1.8% Ti, 0.95 to 2.2% Nb, less than 1.0% Mo, less than 1.0% Mn, up to 0.24% Si, less than 3.0% Fe, less than 0.3% Ta, less than 0.3% W, 0.005 to 0.08% C, 0.01 to 0.3% Zr, 0.0008 to 0.006% B, up to 0.05% rare earth metals, and a balance of Ni plus trace impurities.