- Patent Title: Chemically strengthened glass, and glass for chemical strengthening
-
Application No.: US15920009Application Date: 2018-03-13
-
Publication No.: US10370287B2Publication Date: 2019-08-06
- Inventor: Suguru Murayama , Seiki Ohara , Qing Li , Shusaku Akiba
- Applicant: AGC Inc.
- Applicant Address: JP Tokyo
- Assignee: AGC Inc.
- Current Assignee: AGC Inc.
- Current Assignee Address: JP Tokyo
- Agency: Oblon, McClelland, Maier & Neustadt, L.L.P.
- Priority: JP2016-010002 20160121; JP2016-204745 20161018
- Main IPC: C03C3/085
- IPC: C03C3/085 ; C03C3/097 ; C03C21/00 ; C03C3/087 ; C03C3/083 ; C03C3/091 ; C03C3/093 ; C03C4/18

Abstract:
A glass for chemical strengthening contains, in mole percentage on an oxide basis, 58 to 72% of SiO2, 7 to 18% of Al2O3, 1% or more of B2O3, 0 to 4% of P2O5, 5 to 16% of Li2O, 0 to 7% of Na2O, 0 to 2% of K2O, 0 to 6% of MgO, 0 to 20% of CaO, 0 to 20% of SrO, 0 to 15% of BaO, 0 to 10% of ZnO, 0 to 1% of TiO2, and 0 to 2% of ZrO2. A value of X is 30000 or more. The value of X is calculated based on the formula, X=SiO2×329+Al2O3×786+B2O3×627+P2O5×(−941)+Li2O×927+Na2O×47.5+K2O×(−371)+MgO×1230+CaO×1154+SrO×733+ZrO2×51.8, by using the contents in mole percentage on an oxide basis of components.