Resorbable macroporous bioactive glass scaffold and method of manufacture
Abstract:
A method of manufacturing a resorbable, macroporous bioactive glass scaffold comprising approximately 15-45% CaO, 30-70% SiO2, 0-25% Na2O, 0-17% P2O5, 0-10% MgO and 0-5% CaF2 by mass percent, produced by mixing with pore forming agents and specified heat treatments.