Method for reducing salt usage in aluminum recycling
Abstract:
A method of melting an aluminum charge having no more that 4% salt by mass, including during a melting phase, introducing fuel and oxidant via a burner operating at a first firing rate, the fuel and oxidant reacting to form a combustion zone above the aluminum charge, terminating the melting phase and commencing a transition phase when the aluminum charge is nearly completely molten, during the transition phase, reducing the firing rate of the burner to a second firing rate lower than the first firing rate, introducing a non-oxidizing gas at a first velocity to form a non-oxidizing zone between the combustion zone and the aluminum charge, and allowing the aluminum charge to become completely molten, and terminating the transition phase and commencing a tapping phase after the aluminum charge has become completely molten, and during the tapping phase, pouring the molten aluminum charge out of the furnace.