- Patent Title: Brazing sheet and production method
-
Application No.: US15775428Application Date: 2016-11-09
-
Publication No.: US10730149B2Publication Date: 2020-08-04
- Inventor: Sampath Desikan , Ma Weizeng
- Applicant: GRÄNGES AB
- Applicant Address: SE Stockholm
- Assignee: Gränges AB
- Current Assignee: Gränges AB
- Current Assignee Address: SE Stockholm
- Agency: Morgan, Lewis & Bockius LLP
- Priority: com.zzzhc.datahub.patent.etl.us.BibliographicData$PriorityClaim@42ccdd58 com.zzzhc.datahub.patent.etl.us.BibliographicData$PriorityClaim@3beb756d
- International Application: PCT/EP2016/077057 WO 20161109
- International Announcement: WO2017/081042 WO 20170518
- Main IPC: B23K35/00
- IPC: B23K35/00 ; B23K35/28 ; B23K1/00 ; B32B15/01 ; F28F21/08 ; C22C21/02 ; C22C21/10 ; C22C21/00 ; C22F1/04 ; B23K35/02 ; C22C21/04 ; C22F1/043 ; C22F1/053 ; B21B3/00 ; B23K101/14

Abstract:
Brazing sheet having a core layer made of a first aluminium alloy, attached to one side of said core layer a sacrificial cladding made of a second aluminium alloy, and attached to the other side of said core layer a braze cladding made of a third aluminium alloy. The first aluminium alloy consists of: Si ≤0.6 wt %; Fe ≤0.7 wt %; Cu 0.4-0.9 wt %; Mn 1.0-1.6 wt %; Mg ≤0.2 wt %; Cr 0.05-0.15 wt %; Zr 0.05-0.15 wt %; Ti 0.05-0.15 wt %; other elements ≤0.05 wt % each and ≤0.2 wt % total; Al balance up to 100 wt %; the second aluminium alloy consists of: Si 0.65-1.0 wt %; Fe ≤0.4 wt %; Cu ≤0.05 wt %; Mn 1.4-1.8 wt %; Zn 1.5-4.0 wt %; Zr 0.05-0.20 wt %; other elements ≤0.05 wt % each and ≤0.2 wt % total; Al balance up to 100 wt %. The third aluminium alloy has a melting point lower than said first and second aluminium alloys.