Modified conjugated diene-based polymer and method for producing the same, and modified conjugated diene-based polymer composition
Abstract:
The present invention provides a modified conjugated diene-based polymer, wherein the Mooney stress-relaxation rate measured at 110° C. is 0.45 or less, and the modification percentage is 75% by mass or more.