Ethylene polymer, stretched molded article and microporous membrane
Abstract:
The present invention presents an ethylene polymer, wherein the ethylene polymer has a weight average molecular weight (Mw) of 200,000 or more and 3,000,000 or less, a proportion of a component (α130) with the lowest mobility of 40% or more and 60% or less, and a ratio β/γ of a middle motion component (β) to a component (γ) with the highest mobility of 1.0 or more and 4.0 or less when a three-component approximation of free induction decay at 130° C. measured by a solid echo method of pulse NMR is performed.