- Patent Title: Positive electrode active material for nonaqueous electrolyte secondary battery, and nonaqueous electrolyte secondary battery using the positive electrode active material
-
Application No.: US15771147Application Date: 2016-10-03
-
Publication No.: US10950855B2Publication Date: 2021-03-16
- Inventor: Tetsufumi Komukai , Yuki Furuichi
- Applicant: SUMITOMO METAL MINING CO., LTD.
- Applicant Address: JP Tokyo
- Assignee: SUMITOMO METAL MINING CO., LTD.
- Current Assignee: SUMITOMO METAL MINING CO., LTD.
- Current Assignee Address: JP Tokyo
- Agency: Kratz, Quintos & Hanson, LLP
- Priority: JPJP2015-209492 20151026
- International Application: PCT/JP2016/079303 WO 20161003
- International Announcement: WO2017/073246 WO 20170504
- Main IPC: H01M4/525
- IPC: H01M4/525 ; H01M4/36 ; H01M10/0525 ; H01M4/62 ; C01G53/00 ; H01M4/02

Abstract:
A positive electrode active material for a nonaqueous electrolyte secondary battery is provided, which can establish both high capacity and high output when used for a positive electrode material.
A positive electrode active material for a nonaqueous electrolyte secondary battery comprises primary particles of a lithium-nickel composite oxide represented by the following general formula (1) and secondary particles composed by aggregation of the primary particles, wherein a 1-nm to 200-nm thick film containing W and Li is present on the surface of the primary particles, and a c-axis length in the LiNi composite oxide crystal ranges from 14.183 to 14.205 angstroms. General formula: LibNi1-x-yCoxMyO2 (1) (In the formula, M is at least one type of element selected from Mg, Al, Ca, Ti, V, Cr, Mn, Nb, Zr and Mo, and 0.95≤b≤1.03, 0
A positive electrode active material for a nonaqueous electrolyte secondary battery comprises primary particles of a lithium-nickel composite oxide represented by the following general formula (1) and secondary particles composed by aggregation of the primary particles, wherein a 1-nm to 200-nm thick film containing W and Li is present on the surface of the primary particles, and a c-axis length in the LiNi composite oxide crystal ranges from 14.183 to 14.205 angstroms. General formula: LibNi1-x-yCoxMyO2 (1) (In the formula, M is at least one type of element selected from Mg, Al, Ca, Ti, V, Cr, Mn, Nb, Zr and Mo, and 0.95≤b≤1.03, 0