Heat shrinkable film and preparation method thereof
Abstract:
Embodiments relate to a heat shrinkable film, which has a heat shrinkage rate in the direction perpendicular to the main shrinkage direction that is not high even at a high temperature and which is printable thereon. The heat shrinkable film comprises a polyester resin, wherein the heat shrinkage characteristics in the direction perpendicular to the main shrinkage direction satisfy the following Relationships 1 and 2: −15≤ΔT70−65≤0  [Relationship 1] 0≤ΔT100−95≤5  [Relationship 2] wherein ΔTX−Y is a value obtained by subtracting a heat shrinkage rate of the heat shrinkable film in the direction perpendicular to the main shrinkage direction after the heat shrinkable film is immersed in a water bath for 10 seconds at Y° C. from a heat shrinkage rate of the heat shrinkable film in the direction perpendicular to the main shrinkage direction after the heat shrinkable film is immersed in a water bath for 10 seconds at X° C.