- Patent Title: Copper-nickel-tin alloy, method for the production and use thereof
-
Application No.: US16309701Application Date: 2017-06-27
-
Publication No.: US11041233B2Publication Date: 2021-06-22
- Inventor: Kai Weber
- Applicant: WIELAND-WERKE AG
- Applicant Address: DE Ulm
- Assignee: WIELAND-WERKE AG
- Current Assignee: WIELAND-WERKE AG
- Current Assignee Address: DE Ulm
- Agency: Flynn Thiel, P.C.
- International Application: PCT/EP2017/000758 WO 20170627
- International Announcement: WO2018/014993 WO 20180125
- Main IPC: C22C9/02
- IPC: C22C9/02 ; C22C9/06 ; C22F1/08 ; C22C9/10 ; C21D7/13 ; C21D7/02

Abstract:
A copper-nickel-tin alloy with excellent castability, hot workability and cold workability, high resistance to abrasive wear, adhesive wear and fretting wear and improved resistance to corrosion and stress relaxation stability, consisting of (in weight %): 2.0-10.0% Ni, 2.0-10.0% Sn, 0.01-1.0% Fe, 0.01-0.8% Mg, 0.01-2.5% Zn, 0.01-1.5% Si, 0.002-0.45% B, 0.004-0.3% P, selectively up to a maximum of 2.0% Co, selectively up to a maximum of 0.25% Pb, the residue being copper and unavoidable impurities. The ratio Si/B of the element-contents in wt. % of the elements silicon and boron is a minimum 0.4 and a maximum 8 such that the copper-nickel-tin alloy has Si-containing and B-containing phases, phases of the systems Ni—Si—B, Ni—B, Fe—B, Ni—P, Fe—P, Mg—P, Ni—Si, and Mg—Si, and other Fe-containing phases and Mg-containing phases.