- Patent Title: Welding material for ferritic heat-resistant steel, welded joint for ferritic heat-resistant steel, and method for producing welded joint for ferritic heat-resistant steel
-
Application No.: US16060121Application Date: 2016-12-16
-
Publication No.: US11090755B2Publication Date: 2021-08-17
- Inventor: Hiroyuki Hirata , Kana Jotoku , Tomoaki Hamaguchi , Toshihide Ono , Katsuki Tanaka
- Applicant: NIPPON STEEL & SUMITOMO METAL CORPORATION
- Applicant Address: JP Tokyo
- Assignee: NIPPON STEEL & SUMITOMO METAL CORPORATION
- Current Assignee: NIPPON STEEL & SUMITOMO METAL CORPORATION
- Current Assignee Address: JP Tokyo
- Agency: Clark & Brody LP
- Priority: JPJP2015-246810 20151218
- International Application: PCT/JP2016/087585 WO 20161216
- International Announcement: WO2017/104815 WO 20170622
- Main IPC: B23K9/167
- IPC: B23K9/167 ; C22C38/32 ; C22C38/54 ; C22C38/46 ; C22C38/44 ; C22C38/04 ; C22C38/42 ; C22C38/52 ; C22C38/50 ; C22C38/48 ; B23K9/23 ; B23K35/30 ; C22C38/02 ; C22C38/06 ; C22C38/22 ; C22C38/24 ; C22C38/26 ; C22C38/30

Abstract:
The present invention provides a welding material for ferritic heat-resistant steel, a welded joint for ferritic heat-resistant steel, and a method for producing the welded joint for to form a weld metal having a high creep strength and a high toughness in welding a ferritic heat-resistant steel that contains B. The welding material for ferritic heat-resistant steel has a chemical composition containing, in mass %, C: 0.06 to 0.10%, Si: 0.1 to 0.4%, Mn: 0.3 to 0.7%, Co: 2.6 to 3.4%, Ni: 0.01 to 1.10%, Cr: 8.5 to 9.5%, W: 2.5 to 3.5%, Nb: 0.02 to 0.08%, V: 0.1 to 0.3%, Ta: 0.02 to 0.08%, B: 0.007 to 0.015%, N: 0.005 to 0.020%, with the balance being Fe and impurities, and satisfying Formula (1): 0.5≤Cr+6Si+1.5W+11V+5Nb+10B−40C−30N−4Ni−2Co−2Mn≤10.0 (1).