Invention Grant
- Patent Title: Nonaqueous electrolyte secondary battery
-
Application No.: US15766866Application Date: 2016-09-30
-
Publication No.: US11196078B2Publication Date: 2021-12-07
- Inventor: Kaname Nakajima , Heisuke Nishikawa , Shuji Hitomi
- Applicant: GS Yuasa International Ltd.
- Applicant Address: JP Kyoto
- Assignee: GS Yuasa International Ltd.
- Current Assignee: GS Yuasa International Ltd.
- Current Assignee Address: JP Kyoto
- Agency: Rankin, Hill & Clark LLP
- Priority: JPJP2015-202630 20151014,JPJP2015-218141 20151106,JPJP2016-109738 20160601
- International Application: PCT/JP2016/004426 WO 20160930
- International Announcement: WO2017/064843 WO 20170420
- Main IPC: H01M50/46
- IPC: H01M50/46 ; H01M10/0561 ; H01M10/04 ; H01M10/0568 ; H01M10/058 ; H01M10/0567 ; H01M4/58 ; H01M10/052 ; H01M50/409 ; H01M50/411 ; H01M10/0525 ; H01M4/02

Abstract:
A nonaqueous electrolyte secondary battery includes a sulfur-containing positive electrode, a negative electrode, a nonaqueous electrolyte, and a cation exchange resin layer which is disposed between the positive electrode and the negative electrode and has a first surface having a roughness factor of 3 or more.
A method for producing a nonaqueous electrolyte secondary battery includes a sulfur-containing positive electrode, a negative electrode, and a cation exchange resin layer which is interposed between the positive electrode and the negative electrode and has a first surface having a roughness factor of 3 or more.
The method includes injecting a lithium polysulfide-containing positive electrode electrolyte between the positive electrode and the cation exchange resin layer, and injecting a negative electrode electrolyte between the negative electrode and the cation exchange resin layer, the negative electrode electrolyte having a lithium polysulfide concentration lower than that of the positive electrode electrolyte.
A method for producing a nonaqueous electrolyte secondary battery includes a sulfur-containing positive electrode, a negative electrode, and a cation exchange resin layer which is interposed between the positive electrode and the negative electrode and has a first surface having a roughness factor of 3 or more.
The method includes injecting a lithium polysulfide-containing positive electrode electrolyte between the positive electrode and the cation exchange resin layer, and injecting a negative electrode electrolyte between the negative electrode and the cation exchange resin layer, the negative electrode electrolyte having a lithium polysulfide concentration lower than that of the positive electrode electrolyte.