Abstract:
This polyolefin microporous membrane has a TD thermal shrinkage at 120° C. of 8% or less, and the TD thermal shrinkage at 130° C. thereof is 3 to 5 times greater than the TD thermal shrinkage at 120° C. and at least 12% greater than the TD thermal shrinkage at 120° C.