- Patent Title: Method for producing battery electrode
-
Application No.: US16754828Application Date: 2018-10-10
-
Publication No.: US11329265B2Publication Date: 2022-05-10
- Inventor: Kenichi Toyoshima , Tooru Kosemura , Yuichiro Yokoyama , Yusuke Emori
- Applicant: NISSAN MOTOR CO., LTD.
- Applicant Address: JP Yokohama
- Assignee: NISSAN MOTOR CO., LTD.
- Current Assignee: NISSAN MOTOR CO., LTD.
- Current Assignee Address: JP Yokohama
- Agency: Foley & Lardner LLP
- Priority: JPJP2017-196922 20171010
- International Application: PCT/JP2018/037810 WO 20181010
- International Announcement: WO2019/074024 WO 20190418
- Main IPC: H01M4/04
- IPC: H01M4/04 ; H01M4/36 ; H01M4/62 ; H01M10/0525

Abstract:
Provided is a means capable of improving the flatness of a surface of an electrode active material layer in which an electrode active material slurry without assuming addition of a binder.
Upon producing a battery electrode which has a current collector and an electrode active material layer disposed on a surface of the current collector and containing an electrode active material, in a coating step of coating an electrode active material slurry in which the electrode active material is dispersed in a solvent on the surface of the current collector to form the electrode active material layer, an electrode active material slurry which has flow characteristics that a region A in which a shear stress is not increased according to an increase in shear rate is present and a region B in which a shear stress is increased and an increase rate thereof is decreased according to an increase in shear rate is present in a region having a shear rate larger than that of the region A, in a shear rate (horizontal axis)-shear stress (vertical axis) curve of the electrode active material slurry, is used as the electrode active material slurry, and, coating of the electrode active material slurry is performed at a coating rate at which the shear rate at the time of coating is a value in which a shear stress equal to or more than a yield stress of the electrode active material slurry is applied in the coating step.
Upon producing a battery electrode which has a current collector and an electrode active material layer disposed on a surface of the current collector and containing an electrode active material, in a coating step of coating an electrode active material slurry in which the electrode active material is dispersed in a solvent on the surface of the current collector to form the electrode active material layer, an electrode active material slurry which has flow characteristics that a region A in which a shear stress is not increased according to an increase in shear rate is present and a region B in which a shear stress is increased and an increase rate thereof is decreased according to an increase in shear rate is present in a region having a shear rate larger than that of the region A, in a shear rate (horizontal axis)-shear stress (vertical axis) curve of the electrode active material slurry, is used as the electrode active material slurry, and, coating of the electrode active material slurry is performed at a coating rate at which the shear rate at the time of coating is a value in which a shear stress equal to or more than a yield stress of the electrode active material slurry is applied in the coating step.