Invention Grant
- Patent Title: Method for treating fluorine-containing rare earth mineral particles
-
Application No.: US16630311Application Date: 2019-06-21
-
Publication No.: US11427884B2Publication Date: 2022-08-30
- Inventor: Jianguo Cui , Zhe Wang , Ruien Hou , Dong Li , Meng Xu , Ting Gao , Xiaoli Hao , Bo Li , Yang Zhang
- Applicant: BAOTOU RESEARCH INSTITUTE OF RARE EARTHS , NATIONAL ENGINEERING RESEARCH CENTRE OF RUIKE RARE EARTH METALLURGY AND FUNCTION MATERIALS CO., LTD.
- Applicant Address: CN Baotou; CN Baotou
- Assignee: BAOTOU RESEARCH INSTITUTE OF RARE EARTHS,NATIONAL ENGINEERING RESEARCH CENTRE OF RUIKE RARE EARTH METALLURGY AND FUNCTION MATERIALS CO., LTD.
- Current Assignee: BAOTOU RESEARCH INSTITUTE OF RARE EARTHS,NATIONAL ENGINEERING RESEARCH CENTRE OF RUIKE RARE EARTH METALLURGY AND FUNCTION MATERIALS CO., LTD.
- Current Assignee Address: CN Baotou; CN Baotou
- Agency: Osha, Bergman, Watanabe & Burton LLP
- Priority: CN201811072801.3 20180914
- International Application: PCT/CN2019/092296 WO 20190621
- International Announcement: WO2020/052311 WO 20200319
- Main IPC: C22B3/08
- IPC: C22B3/08 ; C22B59/00

Abstract:
A method for treating fluorine-containing rare earth mineral particles may include mixing a first batch of the fluorine-containing rare earth mineral particles with a first sulfuric acid solution in a weight ratio in the range of 2-10:1 of the sulfuric acid in the first sulfuric acid solution to the first batch of fluorine-containing rare earth mineral particles, and heating the mixture to cause a liquid-solid reaction. The solid phase and liquid phase may be separated after the reaction to obtain an acid filtrate and an acid residue. The acid residue may be leached with water to obtain an aqueous leaching liquor that comprises a rare earth sulfate and an aqueous leaching residue. A second sulfuric acid solution may be added to the acid filtrate in an amount such that the sulfuric acid concentration of the acid filtrate is 40-85 wt %.
Public/Granted literature
- US20210062295A1 METHOD FOR TREATING FLUORINE-CONTAINING RARE EARTH MINERAL PARTICLES Public/Granted day:2021-03-04
Information query