Broad molecular weight distribution polypropylenes with high melt flow rates and high flexural modulus
Abstract:
Provided is a reactor grade polypropylene suitable for injection molding applications comprising within a range from 0 wt % to 4 wt % ethylene and/or C4 to C12 α-olefin derived units, the polypropylene produced from a single catalyst and single stage polymerization process, and having a melt flow rate (MFR, 230° C./2.16 kg) greater than 10 g/10 min, and a 1% secant flexural modulus of at least 250 kpsi (1720 MPa).