- Patent Title: Nickel composite hydroxide and manufacturing method thereof, cathode active material for nonaqueos-electrolyte secondary battery and manufacturing method thereof, and nonaqueous-electrolyte secondary battery
-
Application No.: US17318692Application Date: 2021-05-12
-
Publication No.: US11545663B2Publication Date: 2023-01-03
- Inventor: Atsushi Fukui , Katsuya Inoue , Shuhei Oda , Hiroyuki Toya
- Applicant: SUMITOMO METAL MINING CO., LTD.
- Applicant Address: JP Tokyo
- Assignee: SUMITOMO METAL MINING CO., LTD.
- Current Assignee: SUMITOMO METAL MINING CO., LTD.
- Current Assignee Address: JP Tokyo
- Agency: Katten Muchin Rosenman LLP
- Priority: JPJP2011-127343 20110607
- Main IPC: H01M4/525
- IPC: H01M4/525 ; C01G53/00 ; H01M4/505 ; H01M10/0525 ; H01M4/02

Abstract:
Provided are a cathode active material having a suitable particle size and high uniformity, and a nickel composite hydroxide as a precursor of the cathode active material. When obtaining nickel composite hydroxide by a crystallization reaction, nucleation is performed by controlling a nucleation aqueous solution that includes a metal compound, which includes nickel, and an ammonium ion donor so that the pH value at a standard solution temperature of 25° C. becomes 12.0 to 14.0, after which, particles are grown by controlling a particle growth aqueous solution that includes the formed nuclei so that the pH value at a standard solution temperature of 25° C. becomes 10.5 to 12.0, and so that the pH value is lower than the pH value during nucleation. The crystallization reaction is performed in a non-oxidizing atmosphere at least in a range after the processing time exceeds at least 40% of the total time of the particle growth process from the start of the particle growth process where the oxygen concentration is 1 volume % or less, and with controlling an agitation power requirement per unit volume into a range of 0.5 kW/m3 to 4 kW/m3 at least during the nucleation process.