High-strength reinforcing steel and method for manufacturing same
Abstract:
A method for manufacturing a high-strength steel bar can include the steps of: reheating a steel slab at a temperature ranging from 1000° C. to 1100° C., the steel slab including a certain amount of carbon (C), silicon (Si), manganese (Mn), phosphorus (P), sulfur (S), chromium (Cr), copper (Cu), nickel (Ni), molybdenum (Mo), aluminum (Al), vanadium (V), nitrogen (N), antimony (Sb), tin (Sn), and iron (Fe) and other inevitable impurities, The method can further include finish hot-rolling the reheated steel slab at a temperature of 850° C. to 1000° C., and cooling the hot-rolled steel to a martensite transformation start temperature (Ms (° C.)) through a tempcore process.