Invention Grant
- Patent Title: Method for manufacturing a three-dimensional object
-
Application No.: US16771702Application Date: 2018-12-19
-
Publication No.: US11654615B2Publication Date: 2023-05-23
- Inventor: Stéphane Jeol , Nancy J. Singletary , Ryan Hammonds , Hai Van , David B. Thomas
- Applicant: SOLVAY SPECIALTY POLYMERS USA, LLC
- Applicant Address: US GA Alpharetta
- Assignee: SOLVAY SPECIALTY POLYMERS USA, LLC
- Current Assignee: SOLVAY SPECIALTY POLYMERS USA, LLC
- Current Assignee Address: US GA Alpharetta
- Agency: Osha Bergman Watanabe & Burton LLP
- Priority: EP 157929 2018.02.21
- International Application: PCT/EP2018/086033 2018.12.19
- International Announcement: WO2019/129595A 2019.07.04
- Date entered country: 2020-06-11
- Main IPC: B29C64/118
- IPC: B29C64/118 ; B33Y10/00 ; B33Y30/00 ; B33Y80/00 ; B33Y70/10 ; C08L65/02 ; C08L71/12 ; C08L79/08 ; C08L81/06

Abstract:
A method for manufacturing a three-dimensional (3D) object with an additive manufacturing system, comprising a step consisting in printing layers of the 3D object from the part material comprising a polymeric component comprising, based on the total weight of the polymeric component:
from 5 to 95 wt. % of at least one polymer (P1) comprising at least 50 mol. % of recurring units (R1) consisting of an arylene group comprising at least one benzene ring, each recurring unit (R1) being bound to each other through C—C bonds, wherein the recurring units (R1) are such that, based on the total number of moles of recurring units (R1):less than 90 mol. % are rigid rod-forming arylene units (R1-a), and at least 10 mol. % are kink-forming arylene units (R1-b), and
from 5 to 95 wt. % of at least one polymer (P2), having a glass transition temperature (Tg) between 140° C. and 265° C., and no melting peak, as measured by differential scanning calorimetry (DSC) according to ASTM D3418.
from 5 to 95 wt. % of at least one polymer (P1) comprising at least 50 mol. % of recurring units (R1) consisting of an arylene group comprising at least one benzene ring, each recurring unit (R1) being bound to each other through C—C bonds, wherein the recurring units (R1) are such that, based on the total number of moles of recurring units (R1):less than 90 mol. % are rigid rod-forming arylene units (R1-a), and at least 10 mol. % are kink-forming arylene units (R1-b), and
from 5 to 95 wt. % of at least one polymer (P2), having a glass transition temperature (Tg) between 140° C. and 265° C., and no melting peak, as measured by differential scanning calorimetry (DSC) according to ASTM D3418.