Aluminum-based alloy having improved mechanical strength in ageing at high temperatures and adapted to rapid solidification
Abstract:
The invention relates to an aluminum alloy includes, in mass percentages 3 to 6% titanium, 1.5 to 3% manganese, 1 to 2% iron, 1 to 2% chromium, 0.5 to 1.5% vanadium, 0.5 to 1.5% nickel, 0.2 to 1% zirconium, 0 to 0.5% cerium, 0 to 0.5% lanthanum, the remainder being aluminum and unavoidable impurities.