Invention Publication
- Patent Title: HIGH-STRENGTH THERMAL-STABILITY POLYESTER INDUSTRIAL YARN AND PREPARATION METHOD THEREOF
-
Application No.: US18269968Application Date: 2021-08-25
-
Publication No.: US20240052529A1Publication Date: 2024-02-15
- Inventor: Shanshui WANG , Fangming TANG , Lili WANG , Yiwei SHAO , Yanli ZHAO , Xiaoyu WANG , Chaoming YANG
- Applicant: JIANGSU HENGLI CHEMICAL FIBRE CO., LTD.
- Applicant Address: KR Suzhou
- Assignee: JIANGSU HENGLI CHEMICAL FIBRE CO., LTD.
- Current Assignee: JIANGSU HENGLI CHEMICAL FIBRE CO., LTD.
- Current Assignee Address: CN Suzhou
- Priority: CN 2011602597.9 2020.12.29
- International Application: PCT/CN2021/114425 2021.08.25
- Date entered country: 2023-06-28
- Main IPC: D01F6/84
- IPC: D01F6/84 ; D01F11/08 ; D01D5/08 ; C08G63/183 ; C08G63/685 ; C08G63/80 ; C08G63/91 ; C08G63/86

Abstract:
A high-strength thermal-stability polyester industrial yarn is prepared by spinning, winding and coordination treatment of a modified polyester after a solid-state polycondensation; wherein the method of coordination treatment comprises: soaking the wound fiber in an aqueous solution of a coordination agent, and the concentration of the aqueous solution of the coordination agent is 0.1-0.2 mol/L; wherein the condition of coordination treatment is 48-72 hours at 80-100° C., and the concentration of the aqueous solution of the coordination agent is 0.1-0.2 mol/L; wherein the polyester segments of the prepared high-strength thermal-stability polyester industrial yarn comprises a terephthalic acid segment, an ethylene glycol segment and a 2,6-pyridinedicarboxylic acid segment, and 2,6-pyridinedicarboxylic acid segments of different polyester segments are coordinated by Fe3+, the molar ratio of the terephthalic acid segment to the 2,6-pyridinedicarboxylic acid segment is 1:(0.03-0.05).
Public/Granted literature
- US12077883B2 High-strength thermal-stability polyester industrial yarn and preparation method thereof Public/Granted day:2024-09-03
Information query