Invention Grant
- Patent Title: Martensitic stainless steel and method for manufacturing same
- Patent Title (中): 马氏体不锈钢及其制造方法
-
Application No.: US10443821Application Date: 2003-05-23
-
Publication No.: US07662244B2Publication Date: 2010-02-16
- Inventor: Mitsuru Yoshizawa , Kunio Kondo , Masaaki Igarashi , Yuichi Komizo
- Applicant: Mitsuru Yoshizawa , Kunio Kondo , Masaaki Igarashi , Yuichi Komizo
- Applicant Address: JP Osaka
- Assignee: Sumitomo Metal Industries, Ltd.
- Current Assignee: Sumitomo Metal Industries, Ltd.
- Current Assignee Address: JP Osaka
- Agency: Clark & Brody
- Priority: JP2001-322548 20011019
- Main IPC: C22C38/18
- IPC: C22C38/18

Abstract:
A martensitic stainless steel provided includes C: 0.01-0.1% and Cr: 9-15%, and the retained austenite phase has a thickness not more than 100 nm in such a manner that the X-ray integral intensities of 111γ and 110α satisfy the following formula (a): 0.005≦111γ/(111γ+110α)≦0.05 (a) Such a metal structure can be obtained by the following procedure: the steel is heated at a temperature of the Ac3 point or more, and then cooled from 800° C. to 400° C. at a cooling rate of not less than 0.08° C./sec and further cooled down to 150° C. at a cooling rate of not more than 1° C./sec. The martensitic stainless steel according to the present invention has a relatively high carbon content and a greater toughness in spite of a high mechanical strength, and further exhibits an excellent corrosion resistance, so that it is particularly effective as the material for constructing a deep oil well.