Invention Grant
- Patent Title: Low alloy steel for oil country tubular goods having high sulfide stress cracking resistance
- Patent Title (中): 具有较高硫化物抗应力开裂性能的油管式低合金钢
-
Application No.: US12007165Application Date: 2008-01-07
-
Publication No.: US07670547B2Publication Date: 2010-03-02
- Inventor: Kenji Kobayashi , Tomohiko Omura
- Applicant: Kenji Kobayashi , Tomohiko Omura
- Applicant Address: JP Osaka
- Assignee: Sumitomo Metal Industries, Ltd.
- Current Assignee: Sumitomo Metal Industries, Ltd.
- Current Assignee Address: JP Osaka
- Agency: Clark & Brody
- Priority: JP2005-200682 20050708
- Main IPC: C22C38/00
- IPC: C22C38/00 ; C22C38/60 ; C22C38/22

Abstract:
Low alloy steel for oil country tubular goods contains, in percentage by mass, 0.20% to 0.35% C, 0.05% to 0.5% Si, 0.05% to 0.6% Mn, at most 0.025% P, at most 0.01% S, 0.005% to 0.100% Al, 0.8% to 3.0% Mo, 0.05% to 0.25% V, 0.0001% to 0.005% B, at most 0.01% N, and at most 0.01% O, the balance comprising Fe and impurities, the steel satisfying Expression (1): 12V+1−Mo≧0 (1) where the symbols of elements represent the contents of the elements in percentage by mass. In this way, the steel according to the present invention has high SSC resistance.
Public/Granted literature
- US20080105337A1 Low alloy steel for oil country tubular goods having high sulfide stress cracking resistance Public/Granted day:2008-05-08
Information query