Invention Grant
US07846381B2 Ferritic ductile cast iron alloys having high carbon content, high silicon content, low nickel content and formed without annealing 有权
铁素体球墨铸铁合金,含碳量高,硅含量高,镍含量低,无退火形成

Ferritic ductile cast iron alloys having high carbon content, high silicon content, low nickel content and formed without annealing
Abstract:
Disclosed are methods of making ferritic ductile iron castings (60-40-18) with high toughness (6 ft.lb minimum Charpy V at −20 F and 10 ft.lb minimum Charpy V at +72 F), without adding Nickel and without annealing.