Invention Grant
US07918948B2 Method of production of 780 MPa class high strength steel plate excellent in low temperature toughness
有权
780MPa级高强度钢板的生产方法,具有优异的低温韧性
- Patent Title: Method of production of 780 MPa class high strength steel plate excellent in low temperature toughness
- Patent Title (中): 780MPa级高强度钢板的生产方法,具有优异的低温韧性
-
Application No.: US12734103Application Date: 2009-04-03
-
Publication No.: US07918948B2Publication Date: 2011-04-05
- Inventor: Kazuhiro Fukunaga , Ryuji Uemori , Yoshiyuki Watanabe , Yoshihide Nagai , Rikio Chijiiwa
- Applicant: Kazuhiro Fukunaga , Ryuji Uemori , Yoshiyuki Watanabe , Yoshihide Nagai , Rikio Chijiiwa
- Applicant Address: JP Tokyo
- Assignee: Nippon Steel Corporation
- Current Assignee: Nippon Steel Corporation
- Current Assignee Address: JP Tokyo
- Agency: Kenyon & Kenyon LLP
- Priority: JP2008-101959 20080409; JP2009-061114 20090313
- International Application: PCT/JP2009/057295 WO 20090403
- International Announcement: WO2009/125820 WO 20091015
- Main IPC: C21D8/02
- IPC: C21D8/02

Abstract:
A method of production of 780 MPa class high strength steel plate excellent low temperature toughness comprising heating a steel slab of containing, by mass %, C: 0.06 to 0.15%, Si: 0.05 to 0.35%, Mn: 0.60 to 2.00%, P: 0.015% or less, S: 0.015% or less, Cu: 0.1 to 0.5%, Ni: 0.1 to 1.5%, Cr: 0.05 to 0.8%, Mo: 0.05 to 0.6%, Nb: less than 0.005%, V: 0.005 to 0.060%, Ti: less than 0.003%, Al: 0.02 to 0.10%, B: 0.0005 to 0.003%, and N: 0.002 to 0.006% to 1050° C. to 1200° C. in temperature, hot rolling ending at 870° C. or more, waiting for 10 seconds to 90 seconds, then cooling from 840° C. or more in temperature by a 5° C./s or more cooling rate to 200° C., then tempering at 450° C. to 650° C. in temperature for 20 minutes to 60 minutes.
Public/Granted literature
- US20100206440A1 METHOD OF PRODUCTION OF 780 MPA CLASS HIGH STRENGTH STEEL PLATE EXCELLENT IN LOW TEMPERATURE TOUGHNESS Public/Granted day:2010-08-19
Information query