Invention Grant
- Patent Title: High-strength aluminum alloy extruded product exhibiting excellent corrosion resistance and method of manufacturing same
-
Application No.: US12590475Application Date: 2009-11-09
-
Publication No.: US07927436B2Publication Date: 2011-04-19
- Inventor: Hideo Sano , Yasuaki Yoshino
- Applicant: Hideo Sano , Yasuaki Yoshino
- Applicant Address: JP Minato-ku, Tokyo JP Kobe-shi, Hyogo JP Minato-ku, Tokyo
- Assignee: The Society of Japanese Aerospace Companies,Kawasaki Jukogyo Kabushiki Kaisha,Sumitomo Light Metal Industries, Ltd.
- Current Assignee: The Society of Japanese Aerospace Companies,Kawasaki Jukogyo Kabushiki Kaisha,Sumitomo Light Metal Industries, Ltd.
- Current Assignee Address: JP Minato-ku, Tokyo JP Kobe-shi, Hyogo JP Minato-ku, Tokyo
- Agency: Flynn, Thiel, Boutell & Tanis, P.C.
- Priority: JP2003-103121 20030407
- Main IPC: C22F1/057
- IPC: C22F1/057

Abstract:
The present invention provides a high-strength aluminum alloy extruded product exhibiting excellent corrosion resistance and secondary workability and suitably used as a structural material for transportation equipment such as automobiles, railroad vehicles, and aircrafts, and a method of manufacturing the same. The aluminum alloy extruded product has a composition containing 0.6 to 1.2% of Si, 0.8 to 1.3% of Mg, and 1.3 to 2.1% of Cu while satisfying the following conditional expressions (1), (2), (3) and (4), 3%≦Si %+Mg %+Cu %≦4% (1) Mg %≦1.7×Si % (2) Mg %+Si %≦2.7% (3) Cu %/2≦Mg %≦(Cu %/2)+0.6% (4) and further containing 0.04 to 0.35% of Cr, and 0.05% or less of Mn as an impurity, with the balance being aluminum and unavoidable impurities. The cross section of the extruded product has a recrystallized structure with an average grain size of 500 μm or less.