Invention Grant
- Patent Title: Nickel-laterite process
- Patent Title (中): 镍红土工艺
-
Application No.: US12451229Application Date: 2008-05-01
-
Publication No.: US08016913B2Publication Date: 2011-09-13
- Inventor: William F. Drinkard, Jr.
- Applicant: William F. Drinkard, Jr.
- Applicant Address: US NC Charlotte
- Assignee: Drinkard Metalox, Inc.
- Current Assignee: Drinkard Metalox, Inc.
- Current Assignee Address: US NC Charlotte
- Agent Ralph H. Dougherty
- International Application: PCT/US2008/005608 WO 20080501
- International Announcement: WO2008/137025 WO 20081113
- Main IPC: C22B3/06
- IPC: C22B3/06

Abstract:
An improved method for processing of nickel-bearing ores, laterite ores, saprolite and limonite ores, oxidic and sulfide ores, metallurgical wastes, and other metal-bearing materials, to recover the valuable minerals contained therein, comprising comminuting ore to a desired size; leaching the ore at about 70 C to 130 C for about 30 minutes to 4 hours with nitric acid, raising the temperature of the solution to form a liquid/solid residue in which nickel, cobalt and magnesium values are in solution, and iron, manganese, and aluminum are solid residues in oxide form; conducting a liquid-solid separation and removing the solids; and recovering the nickel, cobalt, and manganese from the liquid-metal concentrate. The leachate is recovered and the nitric acid from the leachate is recycled.