Invention Grant
US08080104B2 Filling material for reinforcing joint and construction method of filling reinforcing joint
有权
用于加固接头的填充材料和填充加固接头的施工方法
- Patent Title: Filling material for reinforcing joint and construction method of filling reinforcing joint
- Patent Title (中): 用于加固接头的填充材料和填充加固接头的施工方法
-
Application No.: US11988282Application Date: 2007-05-22
-
Publication No.: US08080104B2Publication Date: 2011-12-20
- Inventor: Tetsuo Otsuka , Tooru Shiraiwa , Tooru Yagi , Masahiro Abukawa
- Applicant: Tetsuo Otsuka , Tooru Shiraiwa , Tooru Yagi , Masahiro Abukawa
- Applicant Address: JP Tokyo JP Tokyo
- Assignee: Denki Kagaku Kogyo Kabushiki Kaisha,Splice Sleeve Japan, Ltd.
- Current Assignee: Denki Kagaku Kogyo Kabushiki Kaisha,Splice Sleeve Japan, Ltd.
- Current Assignee Address: JP Tokyo JP Tokyo
- Agent Manabu Kanesaka
- Priority: JP2006-279626 20061013
- International Application: PCT/JP2007/060754 WO 20070522
- International Announcement: WO2008/044361 WO 20080417
- Main IPC: C04B14/00
- IPC: C04B14/00 ; C04B18/06 ; C04B14/40 ; C04B24/00

Abstract:
A filler for reinforcement joint that ensures excellent fluidity and retention thereof, exhibiting appropriate length change ratio and high strength performance; and a method of reinforcement joint filling operation using the same. There are provided a filler for reinforcement joint containing a cement, an expanding material, a pozzolana micropowder, a water reducing agent and a sand, and a method of reinforcement joint filling operation using the same, characterized in that the expanding material is a calcium aluminoferrite expanding material, and that the pozzolana micropowder is a silicious micropowder having a silicon dioxide (SiO2) content of 90% or higher and having a hydrogen ion concentration falling in an acid region, and that the water reducing agent is a polycarboxylic acid water reducing agent. The calcium aluminoferrite expanding material preferably has a value of Brain specific surface area of 2000 to 6000 cm2/g. The sand is preferably a weighty sand of 3.0 g/cm3 or higher density.