Invention Grant
US08118953B2 Method for producing steel part having long rolling contact fatigue life
有权
具有滚动接触疲劳寿命长的钢部件的制造方法
- Patent Title: Method for producing steel part having long rolling contact fatigue life
- Patent Title (中): 具有滚动接触疲劳寿命长的钢部件的制造方法
-
Application No.: US12694674Application Date: 2010-01-27
-
Publication No.: US08118953B2Publication Date: 2012-02-21
- Inventor: Takashi Iwamoto , Kunikazu Tomita , Hideto Kimura , Takaaki Toyooka , Hisato Nishisaka , Masao Goto , Hisashi Harada
- Applicant: Takashi Iwamoto , Kunikazu Tomita , Hideto Kimura , Takaaki Toyooka , Hisato Nishisaka , Masao Goto , Hisashi Harada
- Applicant Address: JP JP
- Assignee: JFE Steel Corporation,JTEKT Corporation
- Current Assignee: JFE Steel Corporation,JTEKT Corporation
- Current Assignee Address: JP JP
- Agency: DLA Piper LLP (US)
- Priority: JP2006-052688 20060228
- Main IPC: C21D8/00
- IPC: C21D8/00 ; C21D9/36 ; C21D9/40

Abstract:
A steel part having a long rolling contact fatigue life and capable of further increasing the life of a bearing under severer using condition than usual conditions. The steel part includes steel having a composition containing 0.7% by mass to 1.1% by mass of C, 0.5% by mass to 2.0% by mass of Si, 0.4% by mass to 2.5% by mass of Mn, 1.6% by mass to 5.0% by mass of Cr, 0.1% by mass to less than 0.5% by mass of Mo, 0.010% by mass to 0.050% by mass of Al, less than 0.0015% by mass of Sb as an impurity, and the balance composed of Fe and inevitable impurities, the steel being hardened and tempered. In the steel structure of a portion from the surface to a depth of 5 mm, residual cementite has a grain diameter of 0.05 to 1.5 μm, prior austenite has a grain diameter of 30 μm or less, and the ratio by volume of the residual austenite is less than 25%.
Public/Granted literature
- US20100139819A1 METHOD FOR PRODUCING STEEL PART HAVING LONG ROLLING CONTACT FATIGUE LIFE Public/Granted day:2010-06-10