Invention Grant
- Patent Title: Packaging material for flat electrochemical cell
- Patent Title (中): 用于扁平电化学电池的包装材料
-
Application No.: US12078269Application Date: 2008-03-28
-
Publication No.: US08211568B2Publication Date: 2012-07-03
- Inventor: Takanori Yamashita , Masataka Okushita , Hirohisa Akita , Hiroshi Hoya
- Applicant: Takanori Yamashita , Masataka Okushita , Hirohisa Akita , Hiroshi Hoya
- Applicant Address: JP Shinjuku-ku, Tokyo JP Minato-ku, Tokyo
- Assignee: Dai Nippon Printing Co., Ltd.,Mitsui Chemicals, Inc.
- Current Assignee: Dai Nippon Printing Co., Ltd.,Mitsui Chemicals, Inc.
- Current Assignee Address: JP Shinjuku-ku, Tokyo JP Minato-ku, Tokyo
- Agency: Fitch, Even, Tabin & Flannery, LLP
- Priority: JP2007-091287 20070330; JP2008-077049 20080325
- Main IPC: H01M6/00
- IPC: H01M6/00 ; H01M10/00 ; H01M2/00 ; H01M2/02 ; H01M2/04

Abstract:
In a packaging material for electrochemical cell, a thermally adhesive resin layer is configured of a resin having a propylene based elastomer resin in a propylene based resin. This propylene based elastomer resin is a copolymer composed of a constitutional unit derived from propylene and a constitutional unit derived from an α-olefin having from 2 to 20 carbon atoms; when the total sum of the constitutional unit derived from propylene and the constitutional unit derived from an α-olefin is defined as 100% by mole, contains 50% by mole or more of the constitutional unit derived from propylene; and is satisfied with (a) a Shore A hardness (ASTM D2240) of from 65 to 90, (b) a melting point of from 130 to 170° C., (c) a density (ASTM D1505) of from 860 to 875 kg/m3 and (d) a glass transition temperature as measured by DSC of from −25° C. to −35° C.
Public/Granted literature
- US20080241663A1 Packaging material for flat electrochemical cell Public/Granted day:2008-10-02