Abstract:
A nitriding treatment (Step S6) in which an N content of a decarburization-annealed steel strip is increased is performed between start of a decarburization annealing (Step S4) and occurrence of secondary recrystallization in a finish annealing (Step S5). In hot rolling (Step S1), a silicon steel material is held in a temperature range between 1000° C. and 800° C. for 300 seconds or longer, and then finish rolling is performed.