US08475605B2 Surface layer-hardened steel part and method of manufacturing the same 有权
表面硬化钢部件及其制造方法

Surface layer-hardened steel part and method of manufacturing the same
Abstract:
In the steel for a surface layer hardening which is treated with carburizing in a temperature range of 800° C. to 900° C., chemical composition thereof contains, by mass %, C: 0.10% to 0.60%, Si: 0.01% to 2.50%, Mn: 0.20% to 2.00%, S: 0.0001% to 0.10%, Cr: 2.00% to 5.00%, Al: 0.001% to 0.50%, N: 0.0020% to 0.020%, P: 0.001% to 0.050%, and O: 0.0001% to 0.0030%; the remaining portion thereof includes Fe and unavoidable impurities; and the total amount of Cr, Si, and Mn satisfies, by mass %, 2.0≦Cr+Si+Mn≦8.0.