Invention Grant
US08476324B2 Method for manufacturing anion exchange resin, anion exchange resin, method for manufacturing cation exchange resin, cation exchange resin, mixed bed resin, and method for manufacturing ultrapure water for washing electronic component material 有权
阴离子交换树脂的制造方法,阴离子交换树脂,阳离子交换树脂的制造方法,阳离子交换树脂,混合床树脂,以及制造用于洗涤电子部件材料的超纯水的方法

Method for manufacturing anion exchange resin, anion exchange resin, method for manufacturing cation exchange resin, cation exchange resin, mixed bed resin, and method for manufacturing ultrapure water for washing electronic component material
Abstract:
A method for manufacturing an anion exchange resin, in which remaining of impurities and generation of decomposition products are suppressed and leachables are reduced, the method including the following steps (1-a) to (1-e) of: (1-a) obtaining a cross-linked copolymer by copolymerizing a monovinyl aromatic monomer and a cross-linkable aromatic monomer; (1-b) specifying the content of a specific leachable compound to be 400 μg or less relative to 1 g of the cross-linked copolymer; (1-c) haloalkylating the cross-linked copolymer so as to introduce 80 percent by mole or less of haloalkyl group relative to the monovinyl aromatic monomer; (1-d) removing a specific leachable compound from the haloalkylated cross-linked copolymer; and (1-e) subjecting the haloalkylated cross-linked copolymer to a reaction with an amine compound.
Information query
Patent Agency Ranking
0/0