Invention Grant
- Patent Title: Method for obtaining high-tenacity aramid yarn
- Patent Title (中): 获得高强度芳纶纱的方法
-
Application No.: US12311654Application Date: 2007-11-19
-
Publication No.: US08501071B2Publication Date: 2013-08-06
- Inventor: Hanneke Boerstoel , Johannes Bos , Adriaan Anton Schaap , Dennis Wilbers , Leonardus Antonius Godfried Busscher , Antonius Henricus Maria Schotman , Kurt Rainer Hans-Heinrich Stolze
- Applicant: Hanneke Boerstoel , Johannes Bos , Adriaan Anton Schaap , Dennis Wilbers , Leonardus Antonius Godfried Busscher , Antonius Henricus Maria Schotman , Kurt Rainer Hans-Heinrich Stolze
- Applicant Address: NL Arnhem
- Assignee: Teijin Aramid B.V.
- Current Assignee: Teijin Aramid B.V.
- Current Assignee Address: NL Arnhem
- Agency: Oliff & Berridge, PLC
- Priority: EP06024104 20061121
- International Application: PCT/EP2007/009901 WO 20071119
- International Announcement: WO2008/061668 WO 20080529
- Main IPC: D01F6/00
- IPC: D01F6/00 ; D01F6/905

Abstract:
The invention relates to a method for obtaining high-tenacity aramid yarn, wherein the yarn is made of a copolymer obtained from a mixture of monomers comprising DAPBI, an aromatic para-diamine, and an aromatic para-diacid, wherein the yarn is heated in at least two process steps, characterized in that in a first step the yarn is heated at a temperature of 200 to 360° C. at a tension of at least 0.2 cN/dtex, followed by a second step wherein the yarn is heated at a temperature of 370 to 500° C. at a tension of less than 1 cN/dtex. The invention further pertains to a multifilament aramid yarn spun from a sulfuric acid spin dope and having a tenacity of at least 2500 mN/tex.