Invention Grant
- Patent Title: Process for producing crosslinked fluororubber
- Patent Title (中): 制备交联氟橡胶的方法
-
Application No.: US12160427Application Date: 2006-10-16
-
Publication No.: US08721948B2Publication Date: 2014-05-13
- Inventor: Hiroyuki Sano , Hiroki Matsumoto
- Applicant: Hiroyuki Sano , Hiroki Matsumoto
- Applicant Address: JP Tokyo
- Assignee: NOK Corporation
- Current Assignee: NOK Corporation
- Current Assignee Address: JP Tokyo
- Agency: Crockett & Crockett, PC
- Agent K. David Crockett, Esq.; Niky Economy Syrengelas, Esq.
- Priority: JP2006-004269 20060111
- International Application: PCT/JP2006/320585 WO 20061016
- International Announcement: WO2007/080681 WO 20070719
- Main IPC: B29C71/02
- IPC: B29C71/02

Abstract:
[Problem]To provide a method for producing a polyol-crosslinking, crosslinked fluororubber product which exhibits low tack properties and significantly increased rubber hardness.[Means for Solving the problem] The method comprises pressurizing, heating, and vulcanizing a fluororubber composition to mold a vulcanized product; the fluororubber composition comprising a polyol-crosslinkable fluororubber, a crosslinking accelerator including a quarternary phosphonium salt or a quarternary ammonium salt, and a polyol crosslinking agent, the weight ratio X of the crosslinking accelerator to the polyol crosslinking agent (crosslinking accelerator/polyol crosslinking agent) being from 0.90 to 3.00 for a quarternary phosphonium salt, and being from 0.4 to 0.6 for a quarternary ammonium salt; applying a treatment solution containing the polyol crosslinking agent and the crosslinking accelerator dissohttp://reedman/Manuals/Text_Manual/Section_03.htm - 3.1lved in a solvent to a surface of the vulcanized product; and heat-treating the resulting vulcanized product at a temperature ranging from 200 to 300° C. for 1 to 20 hours.