US08729191B2 Production process of polyacrylic acid (salt) water-absorbent resin
有权
聚丙烯酸(盐)吸水树脂的生产工艺
- Patent Title: Production process of polyacrylic acid (salt) water-absorbent resin
- Patent Title (中): 聚丙烯酸(盐)吸水树脂的生产工艺
-
Application No.: US11883621Application Date: 2006-04-06
-
Publication No.: US08729191B2Publication Date: 2014-05-20
- Inventor: Takaaki Kawano , Hirotama Fujimaru , Kunihiko Ishizaki , Katsuyuki Wada
- Applicant: Takaaki Kawano , Hirotama Fujimaru , Kunihiko Ishizaki , Katsuyuki Wada
- Applicant Address: JP Osaka
- Assignee: Nippon Shokubai Co., Ltd.
- Current Assignee: Nippon Shokubai Co., Ltd.
- Current Assignee Address: JP Osaka
- Agency: Harness, Dickey & Pierce, P.L.C.
- Priority: JP2005-110960 20050407; JP2005-111204 20050407
- International Application: PCT/JP2006/307792 WO 20060406
- International Announcement: WO2006/109842 WO 20061019
- Main IPC: C08F6/02
- IPC: C08F6/02 ; C08F8/44 ; C08F20/06

Abstract:
An embodiment of the present invention allows for production, with a high productivity, of a water-absorbent resin including an improved relationship between absorption capacity and water-soluble polymer which are conflicting properties of the water-absorbent resin, being easily controlled for polymerization reaction, being of no odor, being less colored, and being of high absorption properties. In one embodiment of the present invention, acrylic acid composition is neutralized with a basic composition including an iron content of 0.2 to 5 ppm by weight (relative to a basic compound exclusive of a solvent); and then polymerizing a resultant neutralized product, the acrylic acid composition including: (i) a methoxyphenol content of 10 to 200 ppm by weight relative to the weight of acrylic acid; and (ii) at least one compound content of which is 0 to 10 ppm by weight relative to the weight of acrylic acid, the compound being selected from the group consisting of protoanemonin and furfural.