Invention Grant
US08925349B2 Rare earth ion doped silicate luminescence glass and preparation method thereof
有权
稀土离子掺杂硅酸盐发光玻璃及其制备方法
- Patent Title: Rare earth ion doped silicate luminescence glass and preparation method thereof
- Patent Title (中): 稀土离子掺杂硅酸盐发光玻璃及其制备方法
-
Application No.: US13320753Application Date: 2009-05-19
-
Publication No.: US08925349B2Publication Date: 2015-01-06
- Inventor: Mingjie Zhou , Wenbo Ma , Zhaopu Shi , Yanbo Qiao , Qingtao Li
- Applicant: Mingjie Zhou , Wenbo Ma , Zhaopu Shi , Yanbo Qiao , Qingtao Li
- Applicant Address: CN Shenzhen
- Assignee: Ocean's King Lighting Science & Technology Co., Ltd.
- Current Assignee: Ocean's King Lighting Science & Technology Co., Ltd.
- Current Assignee Address: CN Shenzhen
- International Application: PCT/CN2009/071852 WO 20090519
- International Announcement: WO2010/133025 WO 20101125
- Main IPC: C03C3/095
- IPC: C03C3/095 ; C03C6/04 ; C03B32/00 ; C03C4/12 ; C03C3/062

Abstract:
A rare earth ion doped silicate luminescence glass and preparation method thereof are provided. The luminescence glass is the material with the following formula: aM2O.bM′2O3.cSiO2.dRE2O3, wherein M is at least one of Na, K and Li, M′ is at least one of Y, Gd, La, Sc and Lu, RE is at least one of Ce, Tm, Tb, Ho, Dy, Er, Nd, Sm, Eu and Pr. The preparation method is: grinding the raw material until mixed uniformly, calcining the raw material at 1200-1500° C. for 1-5 h, cooling to room temperature, annealing at 600-1100° C. for 0.5-24 h, cooling to room temperature again, molding then getting the product. The performance of the product is stable. The product is homogenous, and the luminescence performance is good. The light transmittance is high. The process of the preparation method is simple and with low cost.
Public/Granted literature
- US20120061615A1 Rare Earth Ion Doped Silicate Luminescence Glass and Preparation Method Thereof Public/Granted day:2012-03-15
Information query