Invention Grant
US09000096B2 Polyethylene blend composition having a reduced chill roll buildup during extrusion process
有权
聚乙烯共混组合物在挤出过程中累积降低的冷却辊
- Patent Title: Polyethylene blend composition having a reduced chill roll buildup during extrusion process
- Patent Title (中): 聚乙烯共混组合物在挤出过程中累积降低的冷却辊
-
Application No.: US14115948Application Date: 2011-05-27
-
Publication No.: US09000096B2Publication Date: 2015-04-07
- Inventor: Jason C. Brodil , James L. Cooper , Nathan J. Wiker
- Applicant: Jason C. Brodil , James L. Cooper , Nathan J. Wiker
- Applicant Address: US MI Midland
- Assignee: Dow Global Technologies LLC
- Current Assignee: Dow Global Technologies LLC
- Current Assignee Address: US MI Midland
- International Application: PCT/US2011/038347 WO 20110527
- International Announcement: WO2012/166093 WO 20121206
- Main IPC: C08L23/06
- IPC: C08L23/06 ; C08L23/08 ; B32B27/32 ; C08L23/04 ; C08J5/18 ; C08F2/34 ; C08F4/6192

Abstract:
The instant invention provides a polyethylene blend composition having reduced chill roll buildup during extrusion process, and films and coating layers made therefrom. The polyethylene blend composition according to the present invention provide reduced chill roll buildups during extrusion process, and comprises: (a) from 60 to 95 percent by weight of a linear polyethylene composition comprising less than or equal to 100 percent by weight of the units derived from ethylene, and less than 15 percent by weight of units derived from one or more α-olefin comonomers; wherein said linear polyethylene composition has a density in the range of from 0.917 to 0.975 g/cm3, a molecular weight distribution (Mw/Mn) in the range of from 1.70 to 3.62, a melt index (I2) in the range of from 2 to 50 g/10 minutes, and a vinyl unsaturation in the range of from less than 0.06 vinyls per one thousand carbon atoms present in the linear polyethylene composition; and (b) from 5 to 40 percent by weight of a low density polyethylene composition (LDPE) having a density in the range of from 0.915 to 0.930 g/cm3, and a melt index (I2) in the range of from 0.4 to 10; wherein the polyethylene blend composition has a density in the range of 0.917 to 0.960 g/cm3 and a melt index (I2) in the range of from 2 to 30 g/10 minutes.