Invention Grant
US09249043B2 Refractory object and process of forming a glass sheet using the refractory object 有权
使用耐火物体形成玻璃板的耐火材料和工艺

Refractory object and process of forming a glass sheet using the refractory object
Abstract:
A refractory object can include at least approximately 10 wt % Al2O3 and at least approximately 1 wt % SiO2. In an embodiment, the refractory object can include an additive. In a particular embodiment, the additive can include TiO2, Y2O3, SrO, BaO, CaO, Ta2O5, Fe2O3, ZnO, or MgO. The refractory object can include at least approximately 3 wt % of the additive. In an additional embodiment, the refractory object can include no greater than approximately 8 wt % of the additive. In a further embodiment, the creep rate of the refractory object can be at least approximately 1×10−6 h−1. In another embodiment, the creep rate of the refractory object can be no greater than approximately 5×10−5 h−1. In an illustrative embodiment, the refractory object can include a glass overflow trough or a forming block.
Information query
Patent Agency Ranking
0/0