Invention Grant
- Patent Title: Positive electrode active material of power storage device, power storage device, electrically propelled vehicle, and method for manufacturing power storage device
- Patent Title (中): 蓄电装置的正极活性物质,蓄电装置,电动车辆,蓄电装置的制造方法
-
Application No.: US13093050Application Date: 2011-04-25
-
Publication No.: US09318741B2Publication Date: 2016-04-19
- Inventor: Takahiro Kawakami , Masaki Yamakaji
- Applicant: Takahiro Kawakami , Masaki Yamakaji
- Applicant Address: JP Kanagawa-ken
- Assignee: SEMICONDUCTOR ENERGY LABORATORY CO., LTD.
- Current Assignee: SEMICONDUCTOR ENERGY LABORATORY CO., LTD.
- Current Assignee Address: JP Kanagawa-ken
- Agency: Nixon Peabody LLP
- Agent Jeffrey L. Costellia
- Priority: JP2010-103832 20100428; JP2010-104027 20100428; JP2010-104082 20100428
- Main IPC: H01M4/00
- IPC: H01M4/00 ; H01M4/58 ; B82Y30/00 ; H01M4/136 ; H01M4/1397 ; H01M10/0525 ; H01M4/02

Abstract:
An object is to improve the characteristics of a power storage device such as a charging and discharging rate or a charge and discharge capacity. The grain size of particles of a positive electrode active material is nano-sized so that a surface area per unit mass of the active material is increased. Specifically, the grain size is set to greater than or equal to 10 nm and less than or equal to 100 nm, preferably greater than or equal to 20 nm and less than or equal to 60 nm. Alternatively, the surface area per unit mass is set to 10 m2/g or more, preferably 20 m2/g or more. Further, the crystallinity of the active material is increased by setting an XRD half width to greater than or equal to 0.12° and less than 0.17°, preferably greater than or equal to 0.13° and less than 0.16°.
Public/Granted literature