Invention Grant
US09328401B2 Copper alloy casting having excellent machinability, strength, wear resistance and corrosion resistance and method of casting the same
有权
铜合金铸件具有优异的机械加工性,强度,耐磨性和耐腐蚀性及其铸造方法
- Patent Title: Copper alloy casting having excellent machinability, strength, wear resistance and corrosion resistance and method of casting the same
- Patent Title (中): 铜合金铸件具有优异的机械加工性,强度,耐磨性和耐腐蚀性及其铸造方法
-
Application No.: US11573632Application Date: 2005-08-10
-
Publication No.: US09328401B2Publication Date: 2016-05-03
- Inventor: Keiichiro Oishi
- Applicant: Keiichiro Oishi
- Applicant Address: JP Tokyo
- Assignee: MITSUBISHI SHINDOH CO., LTD.
- Current Assignee: MITSUBISHI SHINDOH CO., LTD.
- Current Assignee Address: JP Tokyo
- Agency: Griffin and Szipl PC
- Priority: JP2004-233952 20040810
- International Application: PCT/JP2005/014697 WO 20050810
- International Announcement: WO2006/016629 WO 20060216
- Main IPC: C22C9/04
- IPC: C22C9/04 ; C22C9/02 ; B22D21/02 ; C22C1/06 ; C22C30/02 ; C22C30/06 ; C22F1/08 ; B22D27/00 ; C22C1/03 ; C22C9/00

Abstract:
A copper alloy casting with excellent machinability, strength, wear resistance and corrosion resistance contains Sn: 0.5 to 15 mass %; Zr: 0.001 to 0.049 mass %; P: 0.01 to 0.35 mass %; one or more elements selected from Pb: 0.01 to 15 mass %, Bi: 0.01 to 15 mass %, Se: 0.01 to 1.2 mass %, and Te: 0.05 to 1.2 mass %; and Cu: 73 mass % or more serving as a remainder. In this case, f1=[P]/[Zr]=0.5 to 100, f2=3[Sn]/[Zr]=300 to 15000, and f3=3[Sn]/[P]=40 to 2500 (the content of an element ‘a’ is expressed as [a] mass %). The total content of α, γ and δ-phases is 95% or more, and the mean grain size is 300 μm or less.