- Patent Title: Ferromagnetic particles and process for producing the same, and anisotropic magnet, bonded magnet and compacted magnet
- Patent Title (中): 铁磁颗粒及其制造方法,各向异性磁体,粘结磁体和压实磁体
-
Application No.: US13980703Application Date: 2012-01-19
-
Publication No.: US09378876B2Publication Date: 2016-06-28
- Inventor: Migaku Takahashi , Tomoyuki Ogawa , Yasunobu Ogata , Naoya Kobayashi , Chammika Ruwan Polwatta Gallage , Kaori Kohara
- Applicant: Migaku Takahashi , Tomoyuki Ogawa , Yasunobu Ogata , Naoya Kobayashi , Chammika Ruwan Polwatta Gallage , Kaori Kohara
- Applicant Address: JP Hiroshima JP Sendai
- Assignee: TODA KOGYO CORPORATION,TOHOKU UNIVERSITY
- Current Assignee: TODA KOGYO CORPORATION,TOHOKU UNIVERSITY
- Current Assignee Address: JP Hiroshima JP Sendai
- Agency: Nixon & Vanderhye P.C.
- Priority: JP2011-010695 20110121
- International Application: PCT/JP2012/051075 WO 20120119
- International Announcement: WO2012/099202 WO 20120726
- Main IPC: H01F1/00
- IPC: H01F1/00 ; H01F1/06 ; B22F1/02 ; B22F9/22 ; H01F1/01 ; C22C29/16 ; H01F41/02 ; C01B21/06 ; H01F1/08 ; H01F41/00 ; C22C21/00

Abstract:
Ferromagnetic particles including an Fe16N2 compound phase in an amount of not less than 80% as measured by Mössbauer spectrum and each having an outer shell in which FeO is present in the form of a film having a thickness of not more than 5 nm. Ferromagnetic particles may be made by subjecting iron oxide or iron oxyhydroxide having an average major axis diameter of 40 to 5000 nm and an aspect ratio (major axis diameter/minor axis diameter) of 1 to 200 as a starting material to dispersing treatment to prepare aggregated particles; subjecting the iron compound particles passed through a mesh to hydrogen reducing treatment at a temperature of 160 to 420° C.; and then subjecting the resulting particles to nitridation treatment at a temperature of 130 to 170° C.
Public/Granted literature