Invention Grant
- Patent Title: Aqueous emulsion solution, coloring agent composition containing said aqueous solution, aqueous inkjet ink, and method for producing aqueous emulsion solution
-
Application No.: US14781217Application Date: 2014-04-17
-
Publication No.: US09644106B2Publication Date: 2017-05-09
- Inventor: Hiroyuki Shimanaka , Yoshikazu Murakami , Shinichiro Aoyagi , Sachio Yoshikawa , Mitsuo Yamazaki
- Applicant: DAINICHISEIKA COLOR & CHEMICALS MFG. CO., LTD.
- Applicant Address: JP Tokyo
- Assignee: DAINICHISEIKA COLOR & CHEMICALS MFG. CO., LTD.
- Current Assignee: DAINICHISEIKA COLOR & CHEMICALS MFG. CO., LTD.
- Current Assignee Address: JP Tokyo
- Agency: Hamre, Schumann, Mueller & Larson, P.C.
- Priority: JP2013-089311 20130422
- International Application: PCT/JP2014/060925 WO 20140417
- International Announcement: WO2014/175162 WO 20141030
- Main IPC: C08L53/00
- IPC: C08L53/00 ; C09J7/02 ; A61K9/16 ; C04B35/634 ; C08L33/06 ; C09D11/00 ; C09D11/328 ; C09D17/00 ; C08L33/08 ; C08F293/00 ; C09D153/00 ; C09D11/106 ; C09D11/107 ; C09D11/32 ; C09B67/46 ; C08K5/23 ; C08K5/3417 ; C08K5/3437 ; C09D11/322 ; C09D11/324

Abstract:
A novel aqueous emulsion solution is provided that can be used as a binder for forming a coating film suitable for an inkjet printing system. The present invention is an aqueous emulsion solution containing a polymer I and a polymer II mixed together therein, wherein the polymer I is an A-B block copolymer formed from 90 mass % or more of a methacrylate-based monomer, the A-B block copolymer neutralized with an alkali, a polymer block A is substantially water-insoluble and has a number average molecular weight of 1000 to 10000 and a polydispersity index of 1.5 or less, a polymer block B is synthesized using a monomer containing at least a methacrylic acid and has an acid value of 30 to 250 mgKOH/g, the A-B block copolymer has a number average molecular weight of 5000 to 20000, a content of the polymer block A of 5 to 60% in the A-B block copolymer, and a polydispersity index as a whole of 1.6 or less, the polymer II is a polymer obtained by polymerizing a hydrophobic addition polymerizable monomer and having a glass transition temperature of 70° C. or lower, and further the mass ratio of the polymer I and the polymer II is 5 to 80:95 to 20.