Method for regenerating semi-regenerated reforming catalyst
Abstract:
This disclosure describes a method for regenerating a semi-regenerated reforming catalyst. The method comprises adjusting the reaction temperature to 250-480° C., introducing a sulfur-containing naphtha into the reforming reactor, or stopping introducing a feedstock into the reforming reactor, and introducing a sulfur-containing hydrogen into a recycle gas, until the sulfur content in the catalyst is 0.32-0.8 mass %, then the catalyst is subject to coke-burning, oxychlorination and reduction. Alternatively, the method first subjects the spent catalyst to coke-burning followed by introducing sulfate ions thereinto; and then performing oxychlorination and reduction. Disclosed is still another method for regenerating a platinum-rhenium reforming catalyst, which comprises coke-burning the spent catalyst; introducing sulfur and chlorine in the catalyst by impregnation; and then drying, calcinating and reducing.