Method of manufacturing a vitreous silica crucible having a transparent layer, bubble-containing layers, and a semi-transparent layer in its wall
Abstract:
A method of manufacturing of a vitreous silica crucible includes: fusing silica powder under a reduced pressure of −50 kPa or more and less than −95 kPa to form a transparent vitreous silica layer as an inner layer; fusing silica powder under a reduced pressure of 0 kPa or more and less than −10 kPa to form a bubble-containing vitreous silica layer as an intermediate layer; and fusing silica powder under a reduced pressure of −10 kPa or more and less than −50 kPa to form a semi-transparent vitreous silica layer as an outer layer.